We are a big printing company in Shenzhen China . We offer all book publications, hardcover book printing, papercover book printing, hardcover notebook, sprial book printing, saddle stiching book printing, booklet printing,packaging box, calendars, all kinds of PVC, product brochures, notes, Children's book, stickers, all kinds of special paper color printing products, game cardand so on.
For more information please visit
http://www.joyful-printing.com. ENG only
http://www.joyful-printing.net
http://www.joyful-printing.org
email: info@joyful-printing.net
(1) Reason: Underexposure, the transparency of the positive picture is not good, the light source is aging, and the treatment method: re-make the positive picture, moderately adjust the exposure time: re-test with the gray ladder, extend the exposure time, or replace the light source.
(2) Reason: The glass of the printing machine is a bit dirty, and the adhesive tape is attached to the positive picture. Treatment method: use glass cleaner and film detergent to remove dirt.
(3) Cause: During development, development failure is caused by the adhesion of the water bubbles, and the developer liquid orifice is foamed due to clogging. Treatment: Eliminate the cause of foaming: The developer orifice should be cleaned.
(4) Reason: The hand is not clean when using the PS version (there is fingerprint stain). Treatment method: Keep the mouth and back part of the operation.
(5) Reason: The glue is thin. Treatment method: increase the concentration of the glue.
(6) Reason: The rubber layer is peeled off (when the glue layer is not dry, it is overlapped and stored). Treatment: Do not store under high temperature and high humidity conditions.
(7) Reason: After the end of the plate making, it is kept under high temperature and high humidity conditions. Treatment: Do not store under high temperature and high humidity conditions.
(8) Reason: The developer concentration is too low and the development is not complete. Treatment method: Adjust the developer to the standard concentration.